17-4 PH, 17-4 PH, MIL-C-24111B
17-4 PH, S17400, MIL-C-24527B
17-7 PH, 17-7 PH, MIL-S-25043
301 grades, 301, CSA G110.6
301 grades, 301, FED QQ-S-766D
301 grades, 301, MIL-S-5059D
302/ 303, 302, ASTM A478-97 (302, ASTM A478-97 (ann or bright ann))
302/ 303, 302, FED QQ-S-763F
302/ 303, 302, FED QQ-S-766D
302/ 303, 302, FED QQ-W-423B
302/ 303, 302, MIL-S-862B
302/ 303, 302, MIL-S-5059D
302/ 303, 302, MIL-S-7720A
302/ 303, 303, ASTM A473
302/ 303, 303, MIL-S-862B
302/ 303, 303Se, ASTM A473
302/ 303, 303Se, MIL-S-862B
302/ 303, LH18N9, PN-H-83158 (LH18N9, PN-H-83158 (1))
304, 304, ASTM A908
304, 304, MIL-DTL-23196
304, 304, MIL-S-5059D
304, 304, MIL-S-23195A
304, 304, MIL-S-27419
304, 304, MIL-T-8504B
304, 304, MIL-T-8506A
304, GX8CrNi19-10, DIN SEW 595
304L, 304L, ASME SA688
304L, 304L, FED QQ-S-763F
304L, 304L, FED QQ-S-766D
304L, 304L, MIL-DTL-23196
304L, 304L, MIL-P-1144D
304L, 304L, MIL-S-862B
304L, 304L, MIL-S-4043B
304L, 304L, MIL-S-23195A
304L, 304L, MIL-S-27419
304L, 304L, MIL-T-8606C
304L, 304L, MIL-T-8973
305, 305, ASTM A478-97 (305, ASTM A478-97 (ann or bright ann))
305, 305, FED QQ-S-763F
305, 305, FED QQ-S-766D
309 grades, 309, ASTM A473
309 grades, 309, FED QQ-S-763F
309 grades, 309, FED QQ-S-766D
309 grades, 309, MIL-S-862B
310/ 310H, 310, ASTM A473
310/ 310H, 310, FED QQ-S-763F
310/ 310H, 310, FED QQ-S-766D
310/ 310H, 310, MIL-S-862B
310/ 310H, 310S, ASTM A473
310/ 310H, 310S, FED QQ-S-763F
316, 316, ASME SA688
316, 316, FED QQ-S-763F
316, 316, FED QQ-S-766D
316, 316, MIL-P-1144D
316, 316, MIL-S-862B
316, 316, MIL-S-5059D
316, 316, MIL-S-7720A
316, TS60, ISO 2604-2
316, TS61, ISO 2604-2
316L/316LN, 316L, ASTM A793-96
316L/316LN, 316L, FED QQ-S-763F
316L/316LN, 316L, FED QQ-S-766D
316L/316LN, 316L, MIL-T-8973
316L/316LN, F.3543, UNE 36087/4
317, 317, ASTM A478-97 (317, ASTM A478-97 (ann or bright ann))
317, 317, FED QQ-S-763F
321/ 321H, 321, ASTM A473
321/ 321H, 321, MIL-T-8973
321/ 321H, Ch18N9T, BDS 6738
347/347H/ 348, 347, ASTM A493-95
347/347H/ 348, 347, FED QQ-S-763F
347/347H/ 348, 347, FED QQ-S-766D
347/347H/ 348, 347, MIL-DTL-23196
347/347H/ 348, 347, MIL-P-1144D
347/347H/ 348, 347, MIL-S-862B
347/347H/ 348, 347, MIL-S-23195A
347/347H/ 348, 347, MIL-S-27419
347/347H/ 348, 347, MIL-T-6737C
347/347H/ 348, 347, MIL-T-8606C
347/347H/ 348, 347, MIL-T-8808B
347/347H/ 348, 347, MIL-T-8973
347/347H/ 348, 348, ASTM A473
347/347H/ 348, 348, FED QQ-S-766D
347/347H/ 348, 348, MIL-DTL-23196
347/347H/ 348, 348, MIL-S-23195A
403/ 410, 403, ASTM A479/A479M (403, ASTM A479/A479M (2))
403/ 410, 403, DoD-F-24669/7
403/ 410, 403, FED QQ-S-763F
403/ 410, 403, MIL-S-861
403/ 410, 403, MIL-S-862B
403/ 410, Grade G, DoD-F-24669/8
405, 405, ASTM A473
405, 405, DoD-F-24669/7
405, 405, FED QQ-S-763F
405, 405, MIL-S-861
405, 405, MIL-S-862B
410/ 416, 410, ASTM A479/A479M (410, ASTM A479/A479M (2))
410/ 416, 410, DoD-F-24669/7
410/ 416, 410, FED QQ-S-763F
410/ 416, 410, MIL-S-861
410/ 416, 410, MIL-S-862B
410/ 416, 416, ASTM A473
410/ 416, 416, MIL-S-862B
410/ 416, 416Se, ASTM A473
410/ 416, 416Se, FED QQ-S-763F
410/ 416, 416Se, MIL-S-862B
410/ 416, A, GOST 30208
410/ 416, Grade B Class 1, ASTM A1021
420 grades, 420, ASTM A473
420 grades, 420, FED QQ-S-763F
420 grades, 420, FED QQ-S-766D
420 grades, 420, MIL-S-862B
420 grades, B, GOST 30208
420 grades, C, GOST 30208
429, 429, ASTM A473
429, 429, FED QQ-S-763F
429, 429, FED QQ-S-766D
429, 429, FED QQ-W-423B
429, 429, MIL-S-862B
430, 430, ASTM A473
430, 430, FED QQ-S-763F
430, 430, FED QQ-S-766D
430, 430F, ASTM A473
430, 430F, MIL-S-862B
430, 430FSe, ASTM A473
430, 430FSe, MIL-S-862B
430, S43000, ASTM A493-95 (S43000, ASTM A493-95 (as ann))
431, 431, ASTM A473
431, 431, MIL-S-862B
431, 431, MIL-S-8967
431, 431, MIL-S-18732
440 grades, 440A, ASTM A473
440 grades, 440A, FED QQ-S-763F
440 grades, 440B, ASTM A473
440 grades, 440B, FED QQ-S-763F
440 grades, 440B, MIL-S-862B
440 grades, 440C, ASTM A756-94
440 grades, 440C, FED QQ-S-763F
440 grades, 440C, MIL-B-913
440 grades, 440C, MIL-S-862B
444/ 18-2, 2TiMoCr180, STAS 3583
446, 446, ASTM A473
446, 446, FED QQ-S-763F
446, 446, FED QQ-S-766D
446, 446, MIL-S-862B
446, Ch25T, BDS 6738
1005/ 1006, CS Type B, ASTM A1039/A1039M
1005/ 1006, DS Type A, ASTM A1008/A1008M
1005/ 1006, DS Type B, ASTM A1008/A1008M
1008/ 1009, 1008, FED QQ-S-698
1008/ 1009, 1008, FED QQ-W-461H
1008/ 1009, 1008, MIL-R-8814
1008/ 1009, 1008, MIL-S-11310E
1008/ 1009, 1008, MIL-T-3520
1008/ 1009, 1009, FED QQ-S-698
1008/ 1009, A1n, STAS 9485
1008/ 1009, C1008, FED QQ-S-637A
1008/ 1009, C.0246
1008/ 1009, CR2, SFS 600
1008/ 1009, CR23, ISO 6932
1008/ 1009, CS1008, MIL-S-11310E
1010/ 1011, C1, MIL-S-16788A
1010/ 1011, C10D2, EN 10016/4
1010/ 1011, C10D, EN 10016/2
1010/ 1011, UQSt36, DIN 17111
1012/ 1013, 1012, MIL-R-8814
1012/ 1013, 1012, MIL-S-11310E
1012/ 1013, C.1209
1012/ 1013, CS1012, MIL-S-11310E
1015/ 1016, 1015, DoD-F-24669/1
1015/ 1016, 1015, FED QQ-S-698
1015/ 1016, 1015, FED QQ-W-461H
1015/ 1016, 1015, MIL-S-16974E
1015/ 1016, 1015, MIL-T-3520
1015/ 1016, 1016, DoD-F-24669/1
1015/ 1016, C15, MSZ 31 (C15, MSZ 31 (0-11 mm))
1015/ 1016, C15Mn Grade 1, IS 2100
1015/ 1016, CS 1016, ASTM A1018/A1018M
1015/ 1016, MIL-S-645, MIL-S-645C
1015/ 1016, TS 360, ISO 9329-1
1017/ 1018, 1018 mod, FED QQ-S-698
1018, 1018, FED QQ-S-698
1018, 1018, FED QQ-W-461H
1018, 1018, MIL-R-8814
1018, 1018, MIL-S-11310E
1018, CS1018, MIL-S-11310E
1018, TS5, ISO 2604-2
1019, 1019, FED QQ-S-633A
1019, HT, MIL-S-16113
1019, MIL-R-908, MIL-R-908
1019, MIL-S-7809, MIL-S-7809
1019, MIL-S-20166, MIL-S-20166B
1019, TS 410, ISO 9329-1
1019, TS 430, ISO 9329-1
1019, TW10, ISO 2604-3
1020, 1, MIL-S-10520D
1020, 1020, DoD-F-24669/1
1020, 1020, FED QQ-S-635B
1020, 1020, FED QQ-S-698
1020, 1020, FED QQ-W-461H
1020, 1020, MIL-S-7952A
1020, 1020, MIL-S-11310E
1020, 1020, MIL-T-3520
1020, B, PN-H-92147
1020, C2, MIL-S-16788A
1020, C.1204
1020, C.1205
1020, CS1020, MIL-S-11310E
1020, G10200, MIL-S-46059
1020, M1020, AS 1442
1020, M1020, AS 1443
1020, M1020, ASTM A29/A29M
1020, M1020, ASTM A575-96
1020, M1020, SAE J403
1020, M1020, SP Manual
1022, 1022, DoD-F-24669/1
1022, 1022, MIL-S-11310E
1022, A, PN-H-92147
1022, CS1022, MIL-S-11310E
1022, HSLAS Grade 45 Class 1, ASTM A1011/A1011M
1022, LII450, PN-H-83152
1022, R44, ISO 3304 (R44, ISO 3304 (ann))
1023, M1023, ASTM A29/A29M
1023, M1023, ASTM A575-96
1023, M1023, SAE J403
1023, M1023, SP Manual
1025/ 1026, 6, JIS E1104
1025/ 1026, 1025, MIL-S-7952A
1025/ 1026, 1025, MIL-S-11310E
1025/ 1026, 1025, MIL-T-3520
1025/ 1026, 1025, MIL-T-5066B
1025/ 1026, 1026, MIL-S-22698
1025/ 1026, A, MIL-T-20157
1025/ 1026, B, MIL-T-20157
1025/ 1026, C, MIL-T-20157
1025/ 1026, CG20, UNI 3608 (CG20, UNI 3608 (2))
1025/ 1026, CS1025, MIL-S-11310E
1025/ 1026, D, MIL-T-20157
1025/ 1026, G10250, FED QQ-S-700D
1025/ 1026, HSLAS Grade 55 Class 1, ASTM A1011/A1011M
1025/ 1026, M1025, ASTM A29/A29M
1025/ 1026, M1025, ASTM A575-96
1025/ 1026, M1025, SAE J403
1025/ 1026, M1025, SP Manual
1029, MIL-S-3289B, MIL-S-3289B
1030, 2, MIL-S-10520D
1030, 1030, MIL-S-46070
1030, C3, MIL-S-16788A
1030, C1030, FED QQ-S-635B
1030, C1030, FED QQ-S-700D
1030, CS1030, MIL-S-11310E
1030, E, MIL-T-20157
1030, M1030, AS 1442
1030, M1030, AS 1443
1030, M1031, ASTM A29/A29M
1030, M1031, ASTM A575-96
1030, M1031, SAE J403
1030, M1031, SP Manual
1030, Type V Class H, MIL-S-24093A
1035, 1035, DoD-F-24669/1
1035, 1035, FED QQ-W-461H
1035, 1035, MIL-S-46070
1035, C36, UNI 7847
1035, C1035, FED QQ-S-635B
1035, C1035, FED QQ-S-700D
1035, C.1431
1035, C.1480
1035, Carbon steel, MIL-F-20670B
1035, CFS6, BS 980
1035, Ck35, VSM 10648 (Ck35, VSM 10648 (as roll))
1035, R55, PN-H-84023/01
1040, 1040, DoD-F-24669/1
1040, 1040, FED QQ-S-635B
1040, 1040, MIL-S-46070
1040, C4, MIL-S-16788A
1040, CS1040, AS 1443
1040, CS1040, MIL-S-11310E
1042, C1042, FED QQ-S-635B
1042, C.1500
1045/1045H, 1045, FED QQ-S-700D
1045/1045H, 1045, FED QQ-W-461H
1045/1045H, 1045, MIL-S-46070
1045/1045H, C45G, DIN 17212
1045/1045H, C1045, FED QQ-S-635B
1045/1045H, C.1501
1045/1045H, C.1530
1045/1045H, C.1531
1045/1045H, C.1534
1045/1045H, C.1580
1045/1045H, C.2131
1045/1045H, Class 1, MIL-S-19434B
1045/1045H, Grade A, DoD-F-24669/8
1045/1045H, MIL-S-3039C, MIL-S-3039C
1045/1045H, Type IV Class F, MIL-S-24093A
1045/1045H, Type IV Class G, MIL-S-24093A
1046, 6, AS 1442
1050, 1050, DoD-F-24669/1
1050, 1050, MIL-S-16974E
1050, C5, MIL-S-16788A
1050, C1050, FED QQ-S-635B
1050, C1050, FED QQ-S-700D
1050, C.0745
1050, G10500, MIL-S-46059
1053, MIL-S-20137, MIL-S-20137A
1055, 6, MIL-S-10520D
1055, BY7, GB/T 700
1055, C55E3, AFNOR NF A35-565
1055, C1055, FED QQ-S-700D
1060, 1060, DoD-F-24669/1
1060, 1060, FED QQ-S-633A
1060, 1060, FED QQ-S-00640
1060, 1060, MIL-S-16974E
1060, C6, MIL-S-16788A
1060, C60E, BS EN 10250-2 (C60E, BS EN 10250-2 (norm and norm tempered))
1060, C60E, BS EN 10297-1 (C60E, BS EN 10297-1 (ann))
1060, C60S, BS EN 10132-4 (C60S, BS EN 10132-4_1)
1060, CS60, ISO 4960 (CS60, ISO 4960 (ann))
1060, HS60, BS 1449 Section 1.14 (HS60, BS 1449 Section 1.14 (ann))
1064/ 1065, 3, MIL-S-10520D
1064/ 1065, 5, MIL-S-10520D
1064/ 1065, 1065, MIL-S-46049C
1069/ 1070, 1, MIL-S-11713C
1069/ 1070, 2, MIL-S-11713C
1069/ 1070, C.1833
1069/ 1070, G10700, MIL-B-12504E
1069/ 1070, HS70, BS 1449 Section 1.14
1074/ 1075, 1074, MIL-S-46049C
1074/ 1075, D75K, MSZ 5736
1080, 1080, DoD-F-24669/1
1080, 1080, FED QQ-W-470B
1080, 1080, MIL-S-16974E
1080, C8, MIL-S-16788A
1080, C1080, FED QQ-S-700D
1080, HS80, BS 1449 Section 1.14
1084, 3, IS 4454
1084, C1084, FED QQ-S-700D
1084, FMP82-3, AFNOR NF A35-054
1085, 1085, MIL-S-46049C
1095, 3, MIL-S-11713C
1095, 1095, MIL-S-7947A
1095, 1095, MIL-S-8559A1
1095, 1095, MIL-S-46049C
1095, C10, MIL-S-16788A
1095, C1095, FED QQ-S-700D
1095, HS95, BS 1449 Section 1.14 (HS95, BS 1449 Section 1.14 (ann))
1110, C1110, FED QQ-S-637A
1117, 1117, MIL-S-18411
1117, C1117, FED QQ-S-637A
1118, 1118, FED QQ-S-633A
1118, 1118, FED QQ-S-00643
1118, C1118, FED QQ-S-637A
1118, MIL-S-16124, MIL-S-16124
1118, MIL-S-16611, MIL-S-16611
1118, TStE460, DIN 17102
1137/5020, 1137, FED QQ-S-633A
1137/5020, C1137, FED QQ-S-637A
1137/5020, C.1490 (C.1490 (1))
1137/5020, MIL-S-16124, MIL-S-16124
1139/ 1140, 1141, FED QQ-S-637A
1139/ 1140, C1139, FED QQ-S-637A
1139/ 1140, C1140, FED QQ-S-637A
1139/ 1140, C.0645
1139/ 1140, G11400, ASTM A576-90b
1141, 1141, FED QQ-S-633A
1144, C1144, FED QQ-S-637A
1145/ 1146, C1146, FED QQ-S-637A
1145/ 1146, G11450, ASTM A510/A510M
1151, C1151, FED QQ-S-637A
1211/ 1212, C1211, FED QQ-S-637A
1211/ 1212, C1212, FED QQ-S-637A
1211/ 1212, G12120, ASTM A510/A510M
1213, C1213, FED QQ-S-637A
1213, CF9SMn28, UNI 4838
1215, 1215, FED QQ-S-637A
1215, C.0247
1513, E24-2, AFNOR NF A35-501 (E24-2, AFNOR NF A35-501 (100<t<=150 mm))
1513, FeE 500, ISO 6930-1
1513, HS68F62, BS 1449 Section 1.10
1513, HS75F70, BS 1449 Section 1.10
1513, HSLAS Grade 45 Class 2, ASTM A1008/A1008M
1513, HSLAS Grade 45 Class 2, ASTM A1011/A1011M
1513, HSLAS Grade 45 Class 2, ASTM A1018/A1018M
1513, HSLAS Grade 50 Class 2, ASTM A1008/A1008M
1513, HSLAS Grade 50 Class 2, ASTM A1011/A1011M
1513, HSLAS Grade 50 Class 2, ASTM A1018/A1018M
1513, HSLAS Grade 55 Class 2, ASTM A1008/A1008M
1513, HSLAS Grade 55 Class 2, ASTM A1011/A1011M
1513, HSLAS Grade 60 Class 2, ASTM A1008/A1008M
1513, L245NB, BS EN 10208-2
1513, Q345q-E, GB/T 714 (Q345q-E, GB/T 714 (<=16 mm))
1518, E420D, MSZ 6280 (E420D, MSZ 6280 (3-16 mm))
1518, HS60/55, BS 1449 Section 1.10
1518, HS60F55, BS 1449 Section 1.10
1518, Q345q-D, GB/T 714 (Q345q-D, GB/T 714 (<=16 mm))
1518, Q370q-C, GB/T 714 (Q370q-C, GB/T 714 (<=16 mm))
1518, QStE380N, DIN
1518, TStE355, DIN 17102
1522/1522H, C.0370
1522/1522H, C.0561
1522/1522H, C.0562
1522/1522H, C.0563
1522/1522H, E420 Quality CC, ISO 4951-2
1522/1522H, Grade B, ASTM A588/A588M (Grade B, ASTM A588/A588M (t<=100 mm))
1522/1522H, HSLAS Grade 45 Class 1, ASTM A1018/A1018M
1522/1522H, HSLAS Grade 50 Class 1, ASTM A1011/A1011M
1522/1522H, Q345q-C, GB/T 714 (Q345q-C, GB/T 714 (<=16 mm))
1524/1524H, 6, MIL-S-20145
1524/1524H, 1524, FED QQ-S-633A
1524/1524H, 1524, FED QQ-S-00643
1524/1524H, HSLAS Grade 45 Class 1, ASTM A1008/A1008M
1524/1524H, HSLAS Grade 50 Class 1, ASTM A1008/A1008M
1524/1524H, HSLAS Grade 50 Class 1, ASTM A1018/A1018M
1524/1524H, L3, ASTM A707/A707M
1524/1524H, M540, GB/T 3414 (M540, GB/T 3414 (heat-treated))
1526/1526H, HSLAS Grade 55 Class 1, ASTM A1008/A1008M
1526/1526H, HSLAS Grade 55 Class 1, ASTM A1018/A1018M
1527, C.0551
1527, HSLAS Grade 65 Class 1, ASTM A1011/A1011M
1533/1536, C.0545 (C.0545 (2))
1547, G15470, ASTM A510/A510M
1552, 1552, FED QQ-S-633A
1561, C.0500
1566, 7, MIL-S-10520D
1566, Type II Class 1, FED QQ-W-428B
1566, Type II Class 2, FED QQ-W-428B
1570, VDC, IS 4454/2 (VDC, IS 4454/2 (0.50<d<=0.80 mm))
1580/ 1590, Type I Class 1, FED QQ-W-428B
1580/ 1590, Type I Class 2, FED QQ-W-428B
1580/ 1590, Type II Class 1, FED QQ-W-428B
1580/ 1590, Type II Class 2, FED QQ-W-428B
1580/ 1590, Type III, FED QQ-W-428B
4032/ 4037, FS4032, FED QQ-S-00629
4118/ 4120/ 4121, C23, ASTM A389/A389M
4118/ 4120/ 4121, F22, DoD-F-24669/2
4118/ 4120/ 4121, GX15CrMo5, UNI 3608
4130/ 4135/ 4137, 4130, ASTM A866
4130/ 4135/ 4137, 4130, DoD-F-24669/1
4130/ 4135/ 4137, 4130, MIL-S-16974E
4130/ 4135/ 4137, 4130, MIL-S-18729C
4130/ 4135/ 4137, 4135, ASTM A829/A829M
4130/ 4135/ 4137, 4135, DoD-F-24669/1
4130/ 4135/ 4137, 4135, MIL-S-16974E
4130/ 4135/ 4137, 4135, MIL-S-18733A
4130/ 4135/ 4137, Class B, DoD-F-24669/3
4130/ 4135/ 4137, Class D, DoD-F-24669/3
4130/ 4135/ 4137, G41300, MIL-S-46059
4130/ 4135/ 4137, IC-4130, MIL-S-22141B (IC-4130, MIL-S-22141B (heat-treated))
4130/ 4135/ 4137, IC-4130, MIL-S-22141B (IC-4130, MIL-S-22141B (ann))
4130/ 4135/ 4137, MIL-T-6735, MIL-T-6735A
4130/ 4135/ 4137, MIL-T-6736, MIL-T-6736B
4140/ 4142, 4140, ASTM A866
4140/ 4142, 4140, DoD-F-24669/1
4140/ 4142, 4140, FED QQ-S-626C
4140/ 4142, 4140, MIL-S-5626C
4140/ 4142, Class 3, MIL-S-19434B
4140/ 4142, G41400, MIL-S-46059
4140/ 4142, IC-4140, MIL-S-22141B (IC-4140, MIL-S-22141B (ann))
4140/ 4142, IC-4140, MIL-S-22141B (IC-4140, MIL-S-22141B (heat-treated))
4140/ 4142, IC-Nitralloy 135M, MIL-S-22141B
4145/ 4147, 4145, ASTM A829/A829M
4145/ 4147, 4145, MIL-S-16974E
4145/ 4147, Cr-Mo-V, MIL-B-11595E
4145/ 4147, Type II Class B, MIL-S-24093A
4145/ 4147, Type II Class C, MIL-S-24093A
4145/ 4147, Type II Class D, MIL-S-24093A
4145/ 4147, Type II Class E, MIL-S-24093A
4145/ 4147, Type II Class F, MIL-S-24093A
4150/4150H, ORD 4150 Resulfurized, MIL-B-11595E
4150/4150H, ORD 4150, MIL-B-11595E
4161/4161H, Mn-Cr-Mo, MIL-B-12504E
4340/ E4340, 4340, ASTM A829/A829M
4340/ E4340, 4340, DoD-F-24669/1
4340/ E4340, 4340, FED QQ-S-626C
4340/ E4340, 4340, MIL-S-5000E
4340/ E4340, 4340, MIL-S-8844D
4340/ E4340, 4340, MIL-S-16974E
4340/ E4340, 4340H, SP Manual
4340/ E4340, Class 4, MIL-S-19434B
4340/ E4340, Class 5, MIL-S-19434B
4340/ E4340, Class 6, MIL-S-19434B
4340/ E4340, G43400, MIL-S-46059
4340/ E4340, Type I Class A, MIL-S-24093A
4340/ E4340, Type I Class B, MIL-S-24093A
4340/ E4340, Type I Class C, MIL-S-24093A
4419/ 4520, FP1, ASTM A369A/A369M
4620/ 4621, 4620, ASTM A829/A829M
4620/ 4621, 4620, FED QQ-S-626C
5015, Q345GNHLJ, GB/T 18982
5115/ 5117/ 5120, 5120, SP Manual
5130/ 5132, Cr1Z, MSZ 6251 (Cr1Z, MSZ 6251 (1))
5135/5135H, Cr2, MSZ 61 (Cr2, MSZ 61 (0-16 mm))
6150/6150H, 6150, ASTM A866
6150/6150H, 6150, MIL-S-8503
6150/6150H, CrV2, MSZ 61 (CrV2, MSZ 61 (0-16 mm))
6150/6150H, IC-6150, MIL-S-22141B (IC-6150, MIL-S-22141B (heat-treated))
6150/6150H, IC-6150, MIL-S-22141B (IC-6150, MIL-S-22141B (ann))
6150/6150H, VDCrV-A, ISO 8458-3
8615, 8615, ASTM A829/A829M
8615, 8615, DoD-F-24669/1
8620/ 8720, 8620, ASTM A829/A829M
8620/ 8720, 8620, DoD-F-24669/1
8620/ 8720, 8620, FED QQ-S-626C
8620/ 8720, 8620, MIL-S-8690B
8620/ 8720, 8620, MIL-S-16974E
8622/8622H, 8622, ASTM A829/A829M
8622/8622H, 8622, DoD-F-24669/1
8625/8625H, 8625, ASTM A829/A829M
8625/8625H, 8625, DoD-F-24669/1
8625/8625H, 8625, MIL-S-16974E
8627/8627H, 8627, ASTM A829/A829M
8627/8627H, 8627, DoD-F-24669/1
8630/8630H, 8630, ASTM A829/A829M
8630/8630H, 8630, DoD-F-24669/1
8630/8630H, 8630, MIL-S-6050A
8630/8630H, 8630, MIL-S-16974E
8630/8630H, 8630, MIL-S-18728D
8630/8630H, G86300, MIL-S-46059
8640/ 8740, 8640, ASTM A829/A829M
8640/ 8740, 8640, MIL-S-16974E
8640/ 8740, 8740, ASTM A752/A752M
8640/ 8740, 8740, MIL-S-6049A
8645/ 8650, 8645, ASTM A752/A752M
8645/ 8650, 8645, DoD-F-24669/1
8645/ 8650, 8645, MIL-S-16974E
A27-type casting, 65-35, ASTM A27/A27M
A27-type casting, 70-36, ASTM A27/A27M
Air-hardening medium-alloy cold-work steel, A2, COPANT 337 (A2, COPANT 337 ())
Air-hardening medium-alloy cold-work steel, A2, FED QQ-T-570
Air-hardening medium-alloy cold-work steel, A4, FED QQ-T-570
Air-hardening medium-alloy cold-work steel, A4, NMX-B-082
Air-hardening medium-alloy cold-work steel, A6, COPANT 337
Air-hardening medium-alloy cold-work steel, A6, FED QQ-T-570
Air-hardening medium-alloy cold-work steel, A7, FED QQ-T-570
Air-hardening medium-alloy cold-work steel, A7, NMX-B-082
Air-hardening medium-alloy cold-work steel, A8, FED QQ-T-570
Air-hardening medium-alloy cold-work steel, A8, NMX-B-082
Air-hardening medium-alloy cold-work steel, A9, FED QQ-T-570
Air-hardening medium-alloy cold-work steel, A9, NMX-B-082
Air-hardening medium-alloy cold-work steel, A10, FED QQ-T-570
Air-hardening medium-alloy cold-work steel, A10, NMX-B-082
Boron steel, SWRCHB 531, KS D 3624
CA-15/ CA-40 grades, CA40, ASTM A743/A743M
CA-15/ CA-40 grades, CA-15, MIL-C-24707/6
CA-15/ CA-40 grades, CA-15M, MIL-C-24707/6
CA-15/ CA-40 grades, Class 1, MIL-S-16993A
CA-15/ CA-40 grades, GX20Cr14, DIN EN 10213
CA-15/ CA-40 grades, IC-410, MIL-S-81591
CA-15/ CA-40 grades, IC-440A, MIL-S-81591
CA grades, CA6NM, ASTM A352/A352M
CA grades, CA6NMB, ASTM A487/A487M-93
CA grades, E3N, MIL-C-24707/6
Cast nickel chromium molybdenum steel, 4Q, IS 7899
Cast nickel chromium molybdenum steel, IC-4340, MIL-S-22141B (IC-4340, MIL-S-22141B (heat-treated))
Cast nickel chromium molybdenum steel, IC-4340, MIL-S-22141B (IC-4340, MIL-S-22141B (ann))
Cast nickel chromium molybdenum steel, IC-8620, MIL-S-22141B (IC-8620, MIL-S-22141B (ann))
Cast nickel chromium molybdenum steel, IC-8620, MIL-S-22141B (IC-8620, MIL-S-22141B (heat-treated))
Cast nickel chromium molybdenum steel, IC-8630, MIL-S-22141B (IC-8630, MIL-S-22141B (heat-treated))
Cast nickel chromium molybdenum steel, IC-8630, MIL-S-22141B (IC-8630, MIL-S-22141B (ann))
Cast nickel chromium molybdenum steel, IC-8640, MIL-S-22141B (IC-8640, MIL-S-22141B (heat-treated))
Cast nickel chromium molybdenum steel, IC-8640, MIL-S-22141B (IC-8640, MIL-S-22141B (ann))
Cast nickel chromium molybdenum steel, IC-8735, MIL-S-22141B (IC-8735, MIL-S-22141B (ann))
Cast nickel chromium molybdenum steel, IC-8735, MIL-S-22141B (IC-8735, MIL-S-22141B (heat-treated))
Casting for pressure applications, A1Q, MIL-C-24707/1
Casting for pressure applications, A2Q, ASTM A757/A757M-00
Casting for pressure applications, A2Q, MIL-C-24707/1
Casting for pressure applications, LCC, ASTM A352/A352M
Casting for pressure applications, WCA, MIL-C-24707/1
Casting for pressure applications, WCB, MIL-C-24707/1
Casting for pressure applications, WCC, MIL-C-24707/1
Casting specified by strength, 80-40, ASTM A148/A148M
Casting specified by strength, QQ-S-681F, FED QQ-S-681F
CB grades, IC-17-4, MIL-S-81591
CB grades, IC-431, MIL-S-81591
CD/ CE grades, 4A, ASTM A995/A995M-98
CD/ CE grades, GX2CrNiMoCuN26-5-3-3, ISO 4991
CD/ CE grades, GX2CrNiMoN26-7-4, ISO 4991
CF/ CG grades, CF8A, ASTM A351/A351M
CF/ CG grades, CF10MC, ASTM A351/A351M
CF/ CG grades, CF10SMnN, ACI (SFSA)
CF/ CG grades, CF-8, MIL-C-24707/3
CF/ CG grades, CF-8C, MIL-C-24707/3
CF/ CG grades, CF-8M, MIL-C-24707/3
CF/ CG grades, CG6MMN, ASTM A351/A351M
CF/ CG grades, GX5CrNiMo19-11-2, ISO 4991
CF/ CG grades, I, MIL-S-17509
CF/ CG grades, IC-316, MIL-S-81591
CH grades, Grade 7A, IS 3444
Chromium hot-work steel, GX40CrMoV5-1, DIN 17350
Chromium hot-work steel, H10, FED QQ-T-570
Chromium hot-work steel, H11, FED QQ-T-570
Chromium hot-work steel, H12, FED QQ-T-570
Chromium hot-work steel, H13, FED QQ-T-570
Chromium hot-work steel, H14, FED QQ-T-570
Chromium hot-work steel, H19, FED QQ-T-570
Chromium hot-work steel, T20810, ASTM A681-94
Chromium hot-work steel, VAL105, UNI 2955
Chromium molybdenum steel, 502, ASTM A473
Chromium molybdenum steel, 502, MIL-S-20146
Chromium molybdenum vanadium steel, Grade F, DoD-F-24669/8
Chromium silicon steel, 4340M, MIL-S-83135
Chromium silicon steel, 9262, SP Manual
Chromium steel casting, IC-52100, MIL-S-22141B
Chromium steel casting, L30H, PN-H-83156
CN grades, CN7M, ASTM A743/A743M
Ductile cast iron, 60-42-10, ASTM A716
Ductile cast iron, 60-45-15, MIL-C-24707/5
Ductile cast iron, B, MIL-I-24137
Ductile cast iron, C, MIL-I-24137
Ductile cast iron, D400, SAE J434
Ductile cast iron, D-2, MIL-C-24707/5
Ductile cast iron, D-2C, MIL-C-24707/5
Ductile cast iron, Low Cr-Mo-V-Ti half chill spheroidal graphite, GB/T 1504
Ductile cast iron, Ni-Mo spheroidal graphite, GB/T 1504 (Ni-Mo spheroidal graphite, GB/T 1504 (2))
E9310, 3316, MIL-S-83030A2
E9310, 9310, MIL-S-7393C
E9310, 9310, MIL-S-83030A2
E9310, Class C, DoD-F-24669/3
E9310, Grade D, DoD-F-24669/8
E9310, Grade E, DoD-F-24669/8
E9310, HY-80, MIL-S-16216K (HY-80, MIL-S-16216K (1.25-3 in))
E9310, HY-80, MIL-S-16216K (HY-80, MIL-S-16216K (>3 in))
E9310, HY-80, MIL-S-23009C
E9310, HY-100, MIL-S-16216K
E50100/ E51100/ E52100, 51200, MIL-S-980
E50100/ E51100/ E52100, E51200, MIL-S-7420B
E50100/ E51100/ E52100, E52100, MIL-B-913
E50100/ E51100/ E52100, E52100, MIL-B-81793
Gray cast iron, 300C, ASTM A48/A48M
Gray cast iron, FGL250A, AFNOR NF A32-101 (FGL250A, AFNOR NF A32-101 (20<t<=40 mm))
Gray cast iron, FGL350A, AFNOR NF A32-101 (FGL350A, AFNOR NF A32-101 (20<t<=40 mm))
Gray cast iron, Ni-Resist type, LNC203, AFNOR NF A32-301
High manganese casting, T100MoMn130, STAS 3718
High-carbon high-chromium cold-work steel, D2, FED QQ-T-570
High-carbon high-chromium cold-work steel, D3, FED QQ-T-570
High-carbon high-chromium cold-work steel, D4, FED QQ-T-570
High-carbon high-chromium cold-work steel, D5, FED QQ-T-570
High-carbon high-chromium cold-work steel, D7, FED QQ-T-570
High-carbon nickel chromium steel, LH15, PN-H-84041
HP/ HT grades, GX45NiCrCoW35-25-15-5, ISO 11973
HP/ HT grades, GX50NiCr3525, UNI 3159
Low-alloy tool steel, L2, FED QQ-T-570
Low-alloy tool steel, L6, FED QQ-T-570
Low-alloy tool steel, L7, SAE J438
Low-alloy tool steel, L65HNM, PN-H-83161
Low-carbon high-alloy steel, Grade 95 Category 13-1-0, ISO 13680 (Grade 95 Category 13-1-0, ISO 13680 (Class 2))
Low-carbon nickel chromium steel, 3312, SP Manual
Low-carbon nickel chromium steel, LK37C, MSZ 6259 (LK37C, MSZ 6259 (0-16 mm))
Low-carbon nickel chromium steel, LK45B, MSZ 6259 (LK45B, MSZ 6259 (0-16 mm))
Malleable cast iron, A, MIL-I-24137
Malleable cast iron, M5503, ASTM A602-94
Malleable cast iron, QQ-I-666D, FED QQ-I-666D
Manganese steel, 1330, MIL-S-16974E
Manganese steel, 1335, DoD-F-24669/1
Manganese steel, 1335, MIL-S-16974E
Manganese steel, 1340, MIL-S-16974E
Manganese steel, 1345, FED QQ-S-626C
Manganese steel, H08Mn2MoA, GB/T 12470
Miscellaneous alloy steel, 4B, MIL-C-24707/1
Miscellaneous alloy steel, 14A, MIL-C-24707/1
Miscellaneous alloy steel, 300M, MIL-S-8844D
Miscellaneous alloy steel, 3310, MIL-S-7393C
Miscellaneous alloy steel, 3310, MIL-S-83030A2
Miscellaneous alloy steel, 3316, MIL-S-7393C
Miscellaneous alloy steel, A(128), MIL-C-24707/4
Miscellaneous alloy steel, C1Q, MIL-C-24707/1
Miscellaneous alloy steel, C23, MIL-C-24707/2
Miscellaneous alloy steel, Cr5MoSiV1, GB/T 4223
Miscellaneous alloy steel, CrSiMn, GB/T 4223
Miscellaneous alloy steel, Grades A-G, MIL-F-24669/8
Miscellaneous alloy steel, Hadfield steel modified, MIL-F-24669/4
Miscellaneous alloy steel, MIL-S-866, MIL-S-866C
Miscellaneous alloy steel, MIL-S-7493, MIL-S-7493B (MIL-S-7493, MIL-S-7493B (1))
Miscellaneous alloy steel, MIL-S-7493, MIL-S-7493B (MIL-S-7493, MIL-S-7493B (2))
Miscellaneous alloy steel, MIL-S-46850, MIL-S-46850D (MIL-S-46850, MIL-S-46850D (2))
Miscellaneous alloy steel, MIL-S-46850, MIL-S-46850D (MIL-S-46850, MIL-S-46850D (1))
Miscellaneous alloy steel, MIL-S-46850, MIL-S-46850D (MIL-S-46850, MIL-S-46850D (3))
Miscellaneous alloy steel, Mn-Mo, MIL-B-12504E
Miscellaneous alloy steel, QQ-S-624C, FED QQ-S-624C
Miscellaneous alloy steel, QQ-S-627B, FED QQ-S-627B
Miscellaneous alloy steel, QQ-W-412, FED QQ-W-412
Miscellaneous and special purpose high-alloy steel, Cr20Mn9Ni2Si2N, GB/T 4223
Miscellaneous and special purpose high-alloy steel, Cr21Mn9Ni4N, GB/T 4223
Miscellaneous and special purpose high-alloy steel, Cr22Ni20Co20Mo3W3NbN, GB/T 4223
Miscellaneous and special purpose steels, 65-35, MIL-S-15083
Miscellaneous and special purpose steels, Grade AB, ASTM A521
Miscellaneous and special purpose steels, MIL-S-12505, MIL-S-12505B (MIL-S-12505, MIL-S-12505B (1))
Miscellaneous and special purpose steels, MIL-S-12505, MIL-S-12505B (MIL-S-12505, MIL-S-12505B (2))
Miscellaneous and special purpose steels, QQ-S-630A, FED QQ-S-630A
Miscellaneous and special purpose steels, QQ-S-631A, FED QQ-S-631A
Miscellaneous and special purpose steels, QQ-S-634A, FED QQ-S-634A
Miscellaneous and special purpose steels, QQ-S-692B, FED QQ-S-692B
Miscellaneous and special purpose steels, QQ-S-693B, FED QQ-S-693B
Miscellaneous and special purpose steels, QQ-S-741D, FED QQ-S-741D
Miscellaneous and special purpose steels, QQ-T-830A, FED QQ-T-830A
Miscellaneous and special purpose steels, QQ-W-409A, FED QQ-W-409A
Miscellaneous and special purpose steels, SWP-A, JIS G3522
Miscellaneous casting, 70-36, MIL-S-15083
Miscellaneous casting, 80-40, MIL-S-15083
Miscellaneous casting, CS1040, MIL-S-22146
Miscellaneous casting, IC-1020, MIL-S-22141B (IC-1020, MIL-S-22141B (ann))
Miscellaneous casting, IC-1020, MIL-S-22141B (IC-1020, MIL-S-22141B (casting))
Miscellaneous casting, IC-1020, MIL-S-81591
Miscellaneous casting, IC-1030, MIL-S-22141B (IC-1030, MIL-S-22141B (ann))
Miscellaneous casting, IC-1030, MIL-S-22141B (IC-1030, MIL-S-22141B (casting))
Miscellaneous casting, IC-1030, MIL-S-22141B (IC-1030, MIL-S-22141B (heat-treated))
Miscellaneous casting, IC-1030, MIL-S-81591
Miscellaneous casting, IC-1040, MIL-S-22141B (IC-1040, MIL-S-22141B (heat-treated))
Miscellaneous casting, IC-1040, MIL-S-22141B (IC-1040, MIL-S-22141B (ann))
Miscellaneous casting, IC-1040, MIL-S-22141B (IC-1040, MIL-S-22141B (casting))
Miscellaneous casting, IC-1040, MIL-S-81591
Miscellaneous casting, IC-1050, MIL-S-22141B (IC-1050, MIL-S-22141B (casting))
Miscellaneous casting, IC-1050, MIL-S-22141B (IC-1050, MIL-S-22141B (ann))
Miscellaneous casting, IC-1050, MIL-S-22141B (IC-1050, MIL-S-22141B (heat-treated))
Miscellaneous casting, IC-1050, MIL-S-81591
Miscellaneous casting, WC1, MIL-C-24707/2
Miscellaneous casting, WC6, MIL-C-24707/2
Miscellaneous casting, WC9, MIL-C-24707/2
Miscellaneous chromium molybdenum steel, Class A, DoD-F-24669/3
Miscellaneous chromium molybdenum steel, F11, DoD-F-24669/2
Miscellaneous chromium molybdenum steel, K19526, ASTM A295
Miscellaneous chromium molybdenum steel, TS32, ISO 2604-2
Miscellaneous cold-work steel, F.5125, UNE 36018/2
Miscellaneous ferritic steel, S43932, ASTM A959
Miscellaneous ferritic steel, S44635, ASTM A959
Miscellaneous ferritic steel, TPXM-33, ASTM A268/A268M
Miscellaneous ferritic steel, TPXM-33, ASTM A803/A803M
Miscellaneous high alloy casting, E1Q, MIL-C-24707/1
Miscellaneous high alloy casting, E2N, MIL-C-24707/1
Miscellaneous high alloy casting, E2Q, MIL-C-24707/1
Miscellaneous high alloy casting, HY-80, MIL-S-23008D
Miscellaneous high alloy casting, HY-100, MIL-S-16216K (HY-100, MIL-S-16216K (<=1.25 in))
Miscellaneous high alloy casting, HY-100, MIL-S-16216K (HY-100, MIL-S-16216K (1.25-3 in))
Miscellaneous high alloy casting, HY-100, MIL-S-23008D
Miscellaneous high alloy casting, HY-100, MIL-S-23009C
Miscellaneous high alloy casting, IC-302, MIL-S-81591
Miscellaneous high alloy casting, IC-303, MIL-S-81591
Miscellaneous high alloy casting, IC-304, MIL-S-81591
Miscellaneous high alloy casting, IC-304L, MIL-S-81591
Miscellaneous high alloy casting, IC-310, MIL-S-81591
Miscellaneous high alloy casting, IC-321, MIL-S-81591
Miscellaneous high alloy casting, IC-347, MIL-S-81591
Miscellaneous high alloy casting, IC-416, MIL-S-81591
Miscellaneous high alloy casting, IC-420, MIL-S-81591
Miscellaneous high alloy casting, IC-440C, MIL-S-81591
Miscellaneous high-alloy steel, 202, FED QQ-S-763F
Miscellaneous high-alloy steel, 202, FED QQ-S-766D
Miscellaneous high-alloy steel, 414, ASTM A473
Miscellaneous high-alloy steel, 414, FED QQ-S-763F
Miscellaneous high-alloy steel, 422, ASTM A176-99
Miscellaneous high-alloy steel, 422, DoD-F-24669/7
Miscellaneous high-alloy steel, 422, MIL-S-861
Miscellaneous high-alloy steel, Class 2, MIL-S-19434B
Miscellaneous high-alloy steel, D6, MIL-S-8949
Miscellaneous high-alloy steel, Grade 6, ASTM A289/A289M-97
Miscellaneous high-alloy steel, Grade B, DoD-F-24669/8
Miscellaneous high-alloy steel, Grade C, DoD-F-24669/8
Miscellaneous high-alloy steel, Grade D Class 2, ASTM A1028
Miscellaneous high-alloy steel, GX4CrNi13-4, AFNOR NF A32-054 (GX4CrNi13-4, AFNOR NF A32-054 (100<t<=400 mm))
Miscellaneous high-alloy steel, HY-80, MIL-S-16216K
Miscellaneous high-alloy steel, I (Cr-Ni-P), DoD-F-24669/5
Miscellaneous high-alloy steel, II (Cr-Ni-Mn-P), DoD-F-24669/5
Miscellaneous high-alloy steel, LF3, ASTM A350/A350M
Miscellaneous high-alloy steel, LF5, ASTM A350/A350M (LF5, ASTM A350/A350M (Class 1))
Miscellaneous high-alloy steel, QQ-W-423B, FED QQ-W-423B
Miscellaneous iron alloy, L-NiSiCr3055, MSZ ISO 2892
Miscellaneous iron alloy, QQ-I-652C, FED QQ-I-652C
Miscellaneous iron alloy, QQ-I-653A, FED QQ-I-653A
Miscellaneous low-carbon steel, KL2D, MSZ 1741 (KL2D, MSZ 1741 (0-20 mm))
Miscellaneous nickel chromium molybdenum steel, Grade A Class 1, ASTM A736/A736M
Miscellaneous nickel chromium molybdenum steel, LF787, ASTM A350/A350M (LF787, ASTM A350/A350M (Class 2))
Miscellaneous nickel chromium steel, CrNi, GB/T 4223
Miscellaneous tool steel, T110W6Cr4, IS 3748
Molybdenum high-speed steel, 6W6Mo5Cr4V, GB/T 1299
Molybdenum high-speed steel, H42, FED QQ-T-570
Molybdenum high-speed steel, HS6-5-2-5, AFNOR NF A35-590
Molybdenum high-speed steel, HS6-5-2-5, UNI 2955/5
Molybdenum high-speed steel, HS6-5-2, AFNOR NF A35-590
Molybdenum high-speed steel, HS6-5-2, BS EN ISO 4957
Molybdenum high-speed steel, HS6-5-2, ISO 4957
Molybdenum high-speed steel, HS6-5-2, UNI 2955/5
Molybdenum high-speed steel, HS6-5-2CS, DIN 17350
Molybdenum high-speed steel, HS6-5-2HC, AFNOR NF A35-590
Molybdenum high-speed steel, HS6-5-3-8, BS EN ISO 4957
Molybdenum high-speed steel, HS6-5-3-8, ISO 4957
Molybdenum high-speed steel, HS6-5-3, AFNOR NF A35-590
Molybdenum high-speed steel, HS6-5-3, BS EN ISO 4957
Molybdenum high-speed steel, HS6-5-3, ISO 4957
Molybdenum high-speed steel, HS6-5-3, UNI 2955/5
Molybdenum high-speed steel, HS6-5-3C, BS EN ISO 4957
Molybdenum high-speed steel, HS6-5-3C, ISO 4957
Molybdenum high-speed steel, HS6-5-4-2, AFNOR NF A35-590
Molybdenum high-speed steel, HS6-5-4, AFNOR NF A35-590
Molybdenum high-speed steel, HS6-5-4, BS EN ISO 4957
Molybdenum high-speed steel, HS6-5-4, ISO 4957
Molybdenum high-speed steel, HS6-6-2, BS EN ISO 4957
Molybdenum high-speed steel, HS6-6-2, ISO 4957
Molybdenum high-speed steel, HS7-4-2-5, AFNOR NF A35-590
Molybdenum high-speed steel, HS7-4-2-5, UNI 2955/5
Molybdenum high-speed steel, HS7-5-5-5, AFNOR
Molybdenum high-speed steel, HS7-6-3-12, AFNOR NF A35-590
Molybdenum high-speed steel, HS-6-5-2, DIN 17350
Molybdenum high-speed steel, HS-6-5-2S, DIN 17350
Molybdenum high-speed steel, HS-6-5-3, DIN 17350
Molybdenum high-speed steel, HS-7-4-2-5, DIN 17350
Molybdenum high-speed steel, HSC6-5-3, UNI 2955/5
Molybdenum high-speed steel, M1, FED QQ-T-590C
Molybdenum high-speed steel, M2 high C, FED QQ-T-590C
Molybdenum high-speed steel, M2, FED QQ-T-590C
Molybdenum high-speed steel, M3-1, FED QQ-T-590C
Molybdenum high-speed steel, M3-2, FED QQ-T-590C
Molybdenum high-speed steel, M4, FED QQ-T-590C
Molybdenum high-speed steel, M6, FED QQ-T-590C
Molybdenum high-speed steel, M7, FED QQ-T-590C
Molybdenum high-speed steel, M10 high C, FED QQ-T-590C
Molybdenum high-speed steel, M10, FED QQ-T-590C
Molybdenum high-speed steel, M30, FED QQ-T-590C
Molybdenum high-speed steel, M33, FED QQ-T-590C
Molybdenum high-speed steel, M34, FED QQ-T-590C
Molybdenum high-speed steel, M36, FED QQ-T-590C
Molybdenum high-speed steel, M41, FED QQ-T-590C
Molybdenum high-speed steel, M42, FED QQ-T-590C
Molybdenum high-speed steel, M46, FED QQ-T-590C
Molybdenum steel casting, IC-4335M, MIL-S-22141B (IC-4335M, MIL-S-22141B (heat-treated))
Molybdenum steel casting, IC-4335M, MIL-S-22141B (IC-4335M, MIL-S-22141B (ann))
Nickel chromium alloy, CK-3MN, ACI (SFSA)
Nickel steel casting, GX40NiCrSi35-17, ISO 11973
Nickel steel casting, IC-4620, MIL-S-22141B (IC-4620, MIL-S-22141B (ann))
Nickel steel casting, IC-4620, MIL-S-22141B (IC-4620, MIL-S-22141B (heat-treated))
Nickel steel casting, N7M, ASTM A494/A494M
Nickel steel, Type III Class D, MIL-S-24093A
Nickel steel, Type III Class E, MIL-S-24093A
Nickel steel, Type III Class F, MIL-S-24093A
Nickel-base alloy, 330C12, BS 3100
Nickel-base alloy, V-57, SAE J467
Oil-hardening cold-work steel, O1, FED QQ-T-570
Oil-hardening cold-work steel, O2, FED QQ-T-570
Oil-hardening cold-work steel, O6, FED QQ-T-570
Oil-hardening cold-work steel, O7, FED QQ-T-570
PS59/ PS64/ PS65, Q355NH, GB/T 4172 (Q355NH, GB/T 4172 (<=16 mm))
Shock-resisting steel, S-1, FED QQ-T-570
Shock-resisting steel, S-2, FED QQ-T-570
Shock-resisting steel, S-5, FED QQ-T-570
Shock-resisting steel, S-6, FED QQ-T-570
Shock-resisting steel, S-7, FED QQ-T-570
Silicon steel, C.2132
Tungsten high-speed steel, HS18-0-1-10, UNI 2955/5
Tungsten high-speed steel, T1, FED QQ-T-590C
Tungsten high-speed steel, T4, FED QQ-T-590C
Tungsten high-speed steel, T5, FED QQ-T-590C
Tungsten high-speed steel, T6, FED QQ-T-590C
Tungsten high-speed steel, T8, FED QQ-T-590C
Tungsten high-speed steel, T15, FED QQ-T-590C
Tungsten high-speed steel, T15, NMX-B-082
Tungsten hot-work steel, H21, FED QQ-T-570
Tungsten hot-work steel, H22, FED QQ-T-570
Tungsten hot-work steel, H23, FED QQ-T-570
Tungsten hot-work steel, H24, FED QQ-T-570
Tungsten hot-work steel, H26, FED QQ-T-570
Tungsten hot-work steel, VCW85, STAS 3611
Water-hardening type steel, N9, PN-H-85020
Water-hardening type steel, N11, PN-H-85020
Water-hardening type steel, N13E, PN-H-85020
Water-hardening type steel, W2, FED QQ-T-580C
White Cast Iron, CrMoLC28/500, IS 4771 (CrMoLC28/500, IS 4771 (ann))
White Cast Iron, G-X260NiCr42, DIN
White Cast Iron, NiLCr34/550, IS 4771
XM-15, TPXM-15, ASTM A943/A943M
XM-19, TPXM-19, ASTM A249/A249M
XM-19, TPXM-19, ASTM A269
XM-19, TPXM-19, ASTM A312/A312M
XM-19, TPXM-19, IS 11714/5
XM-29, TPXM-29, ASTM A688/A688M
XM-29, TPXM-29, ASTM A813/A813M
XM-29, TPXM-29, ASTM A814/A814M
XM-29, TPXM-29, ASTM A943/A943M
UNHANDLED ERROR!
View log for stack trace
Close
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch record
Add to list
Copy to clipboard
Watch folder
Download Excel Template
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch generic
Download Excel Template
Add to list
Copy to clipboard
Watch table
Download Excel Template
Add all results from this table to list
Copy all results from this table to clipboard
Watch table
Add to list
Copy to clipboard
Find substitutes for this record
Watch record
Add all to list
Copy all to clipboard
Add all to list
Copy all to clipboard