Chemical Composition
0.07
%  (maximum)  
14 to 15.5
%    
2.5 to 3.2
%    
0.7
%  (maximum)  
0.05
%  (maximum)  
0.15 to 0.35
%    
4.5 to 5.5
%    
0.035
%  (maximum)  
0.03
%  (maximum)  
1
%  (maximum)  
 
Mechanical Properties
DimensionsYield Strength (MPa)Ultimate Tensile Strength (MPa)Elongation (% strain)Brinell Hardness
None Specified≥ 669≥ 862≥ 10≥ 269

669
MPa  (minimum)  
862
MPa  (minimum)  
10
% strain  (minimum)  
269
 (minimum)  
 
Other Information
Links
 



No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®