Chemical Composition
0.03
%  (maximum)  
18 to 20
%    
63.9 to 73
%    (estimate)
2
%  (maximum)  
9 to 13
%    
0.045
%  (maximum)  
0.03
%  (maximum)  
1
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
175
MPa  (minimum)  
480
MPa  (minimum)  
40
% strain  (minimum)  
187
 (minimum)  
 
Other Information



No warranty is given for the accuracy of these data