Chemical Composition
0.02
%  (minimum)  
0.2
%  (maximum)  
0.3
%  (maximum)  
0.35
%  (maximum)  
96.1 to 99.1
%    (estimate)
0.9 to 1.65
%    
0.1
%  (maximum)  
0.015
%  (maximum)  
0.05
%  (maximum)  
0.5
%  (maximum)  
0.035
%  (maximum)  
0.03
%  (maximum)  
0.5
%  (maximum)  
0.03
%  (maximum)  
0.12
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
Not Applicable
345
MPa  (minimum)  
470 to 630
MPa    
22
% strain  (minimum)  
 
Other Information
Links



No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®