Chemical Composition
0.015
%  (minimum)  
0.2
%  (maximum)  
0.7
%  (maximum)  
95.6 to 98.9
%    (estimate)
1 to 1.7
%    
0.015 to 0.06
%    
0.7
%  (maximum)  
0.03
%  (maximum)  
0.03
%  (maximum)  
0.55
%  (maximum)  
0.02 to 0.2
%    
0.02 to 0.2
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
Not Applicable
400 to 460
MPa    
550 to 720
MPa    
12
% strain  (minimum)  
 