Chemical Composition
0.85 to 0.95
%    
0.35
%  (maximum)  
96 to 97.5
%    (estimate)
1.4 to 1.8
%    
0.3
%  (maximum)  
0.2 to 0.4
%    
0.2
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
Other Information
Oil-hardening cold-work tool steels
EN ISO 4957:1999, NF EN ISO 4957:2, DIN EN ISO 4957:21, UNI EN ISO 4957:22, UNE EN ISO 4957:2, BS EN ISO 4957:2, ISO 4957:1999, JIS G 444:215, JIS G 771:2, ASTM A681 - 8(215)
 