Chemical Composition
0.35 to 0.4
%    
0.8 to 1.1
%    
96.9 to 97.9
%    (estimate)
0.7 to 0.9
%    
0.15 to 0.25
%    
0.035
%  (maximum)  
0.04
%  (maximum)  
0.15 to 0.35
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
725
MPa  (minimum)  
860
MPa  (minimum)  
16
% strain  (minimum)  
 
Other Information
Links