Chemical Composition
0.02
%  (maximum)  
19 to 21
%    
1 to 2
%    
42.9 to 51.5
%    (estimate)
2
%  (maximum)  
4.5 to 5.5
%    
24 to 26
%    
0.02
%  (maximum)  
0.015
%  (maximum)  
0.5
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
220
MPa    
500 to 700
MPa    
35
% strain    
190
 (maximum)  
 
Other Information