Chemical Composition
0.85 to 0.95
%    
3.6 to 4.3
%    
85.2 to 89
%    (estimate)
0.4
%  (maximum)  
4.1 to 4.8
%    
0.03
%  (maximum)  
0.03
%  (maximum)  
0.65
%  (maximum)  
1.7 to 2.2
%    
0.8 to 1.4
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
Other Information
High-speed tool steel.
EN ISO 4957:1999, NF EN ISO 4957:2, DIN EN ISO 4957:21, UNI EN ISO 4957:22, UNE EN ISO 4957:2, BS EN ISO 4957:2, JIS G 443:215, JIS G 771:2, ASTM A6:1992a(216), SAE J438:197,
 