Chemical Composition
0.25 to 0.35
%    
23 to 27
%    
47.3 to 57.8
%    (estimate)
1.5
%  (maximum)  
19 to 22
%    
0.04
%  (maximum)  
0.04
%  (maximum)  
1.75
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
235
MPa  (minimum)  
440
MPa  (minimum)  
8
% strain  (minimum)  
 