Chemical Composition
0.02
%  (maximum)  
0.0007
%  (maximum)  
0.1
%  (maximum)  
0.25
%  (maximum)  
0.35
%  (maximum)  
96 to 98.9
%    (estimate)
0.92 to 1.72
%    
0.33
%  (maximum)  
0.05
%  (maximum)  
0.6
%  (maximum)  
0.015
%  (maximum)  
0.006
%  (maximum)  
0.15 to 0.5
%    
0.08
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
485
MPa  (minimum)  
585 to 724
MPa    
20
% strain  (minimum)  
 
Other Information
Links



No warranty is given for the accuracy of these data