Chemical Composition
0.0007
%  (maximum)  
0.08 to 0.12
%    
2.8 to 3.2
%    
92.8 to 94.5
%    (estimate)
0.25 to 0.45
%    
0.65 to 0.85
%    
0.25
%  (maximum)  
0.01
%  (maximum)  
0.01
%  (maximum)  
0.15 to 0.4
%    
0.2 to 0.3
%    
1.35 to 1.65
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
585
MPa  (minimum)  
725 to 930
MPa    
16
% strain  (minimum)  
 
Other Information