Layout: Alloy Finder
View
Full datasheet
Printable datasheet
Show empty items
Record properties
Expand headings
Collapse headings
Change layout
No layout
~Release Layout
Alloy Finder (Default)
Explore Chemical Composition
Explore Properties
Tools
Add to list
Copy to clipboard
Export to text file…
Export to Excel…
Find substitutes for this record
View related records
Watch data…
Watch this record
Bookmark
Units
Metric
CGS (Consistent)
FPS (Consistent)
IPS (Consistent)
SI (Consistent)
UK Imperial
US Customary
S21900 Grade TPXM-10, ASME SA814/SA814M, Pipe
add data link
Chemical Composition
Base Element
Fe (Iron)
C (Carbon)
0.08
% (maximum)
Cr (Chromium)
19 to 21.5
%
Mn (Manganese)
8 to 10
%
N (Nitrogen)
0.15 to 0.4
%
Ni (Nickel)
5.5 to 7.5
%
P (Phosphorus)
0.045
% (maximum)
S (Sulfur)
0.03
% (maximum)
Si (Silicon)
1
% (maximum)
Mechanical Properties
Tabular Data
Hide table
Save as CSV
Copy To Clipboard
Dimensions
Yield Strength (MPa)
Ultimate Tensile Strength (MPa)
None Specified
≥ 379
≥ 689
Save as CSV
Copy To Clipboard
Yield Strength
379
MPa (minimum)
Ultimate Tensile Strength
689
MPa (minimum)
Other Information
Material Class
Ferrous Alloy
Alloy Family
High-Alloy Steel (Corrosion and Heat Resistant, Stainless, and Nickel Steels)
Alloy Group
Austenitic stainless steel
Alloy Sub-Group
XM-10
Country
USA
Standards Body
ASME (USA)
Description
Single- or Double-welded austenitic stainless steel pipe
Designation
S21900 Grade TPXM-10
Specification Type
Standard
Specification
ASME SA813/SA813M
Specification Year
2011
Specification Status
Active
Similar US Grade
S21900
Similar UNS Number
S21900
Source
BPVC Section II-Materials-Part A-Ferrous Materials Specifications
Organization
ASME International (ASME)
Available forms
Pipe
Similar Alloys
Click here to find similar alloys
Links
Organizations
ASME International (ASME)
No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®
UNHANDLED ERROR!
View log for stack trace
Close
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch record
Add to list
Copy to clipboard
Watch folder
Download Excel Template
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch generic
Download Excel Template
Add to list
Copy to clipboard
Watch table
Download Excel Template
Add all results from this table to list
Copy all results from this table to clipboard
Watch table
Add to list
Copy to clipboard
Find substitutes for this record
Watch record
Add all to list
Copy all to clipboard
Add all to list
Copy all to clipboard