Chemical Composition
0.11
%  (maximum)  
0.2
%  (maximum)  
0.5
%  (maximum)  
95.8 to 97.5
%    (estimate)
1.8 to 2.1
%    
0.3
%  (maximum)  
0.03
%  (maximum)  
0.03
%  (maximum)  
0.65 to 0.95
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
3.72e8
Pa  (minimum)  
4.9e8
Pa  (minimum)  
20
% strain  (minimum)  
 
Other Information