Chemical Composition
0.47 to 0.55
%    
0.4
%  (maximum)  
0.3
%  (maximum)  
96.9 to 98.8
%    (estimate)
0.6 to 0.9
%    
0.1
%  (maximum)  
0.4
%  (maximum)  
0.045
%  (maximum)  
0.045
%  (maximum)  
0.1 to 0.4
%    
Cr + Mo + Ni ≤ 0.63 %
1) Cast analysis.
2) The steel shall be supplied in the fully killed condition.
3) Steels may be supplied with a lower silicon content. In this case, alternative means of deoxidation shall be used.
4) Steels with improved machinability either by higher S levels up to about 0.10 % S (including controlled sulfide morphology) or Pb additions may be supplied on request. In the first case, the upper limit for the Mn content may be increased by 0.15 %.
5) Cu content above 0.40 % can cause hot shortness during hot forming.
6) Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
DimensionsUltimate Tensile Strength (MPa)Brinell Hardness
Thickness, > 16 to ≤ 40 mm610 to 910179 to 269
Thickness, > 40 to ≤ 63 mm610 to 910179 to 269
Thickness, > 63 to ≤ 100 mm610 to 910179 to 269

610 to 910
MPa    
179 to 269
   
As-rolled, peeled (+SH)
 
Other Information
Links



No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®