Chemical Composition
0.32 to 0.39
%    
0.4
%  (maximum)  
97.4 to 99.2
%    (estimate)
0.5 to 0.8
%    
0.1
%  (maximum)  
0.4
%  (maximum)  
0.035
%  (maximum)  
0.035
%  (maximum)  
0.4
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
300
MPa  (minimum)  
500 to 650
MPa    
20
% strain  (minimum)  
 
Other Information