Chemical Composition
0.22 to 0.29
%    
98.5 to 99.4
%    (estimate)
0.4 to 0.7
%    
0.035
%  (maximum)  
0.02 to 0.035
%    
0.4
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
370
MPa    
550 to 700
MPa    
19
% strain    
 
Other Information