Chemical Composition
0.27 to 0.34
%    
0.6 to 0.9
%    
0.3
%  (maximum)  
94.3 to 96.2
%    (estimate)
0.35 to 0.6
%    
2.5 to 3
%    
0.035
%  (maximum)  
0.035
%  (maximum)  
0.1 to 0.4
%    
0.05
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
850
MPa    
1030 to 1230
MPa    
11
% strain    
 
Other Information
Links