Chemical Composition
0.2
%  (maximum)  
0.2
%  (maximum)  
0.3
%  (maximum)  
96.5 to 100
%    (estimate)
1.7
%  (maximum)  
0.1
%  (maximum)  
0.01 to 0.06
%    
0.2
%  (maximum)  
0.03
%  (maximum)  
0.02
%  (maximum)  
0.5
%  (maximum)  
0.05
%  (maximum)  
0.02 to 0.15
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
440
MPa    
590 to 700
MPa    
17
% strain    
 