Chemical Composition
0.48 to 0.53
%    
0.4 to 0.6
%    
96.5 to 97.5
%    (estimate)
0.75 to 1
%    
0.15 to 0.25
%    
0.4 to 0.7
%    
0.04
%    
0.04
%    
0.2 to 0.35
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 