Chemical Composition
0.35 to 0.45
%    
3 to 3.5
%    
93.3 to 95.1
%    (estimate)
0.4 to 0.7
%    
0.9 to 1.1
%    
0.3
%  (maximum)  
0.1 to 0.35
%    
0.15 to 0.25
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
1050
MPa  (minimum)  
1340
MPa  (minimum)  
8
% strain  (minimum)  
363
 (minimum)  
 