Chemical Composition
0.0005
%  (minimum)  
0.56 to 0.64
%    
0.4 to 0.6
%    
0.35
%  (maximum)  
96.7 to 98.1
%    (estimate)
0.75 to 1
%    
0.06
%  (maximum)  
0.25
%  (maximum)  
0.035
%  (maximum)  
0.04
%  (maximum)  
0.15 to 0.3
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
710
MPa  (maximum)  
 
Other Information
Links



No warranty is given for the accuracy of these data