Chemical Composition
0.0003
%  (maximum)  
0.4 to 0.5
%    
8.5 to 9.5
%    
0.35
%  (maximum)  
85.3 to 88.1
%    (estimate)
0.3 to 0.6
%    
0.05
%  (maximum)  
0.25
%  (maximum)  
0.035
%  (maximum)  
0.035
%  (maximum)  
2.75 to 3.25
%    
0.05
%  (maximum)  
0.05
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
685
MPa  (minimum)  
880 to 1030
MPa    
10
% strain  (minimum)  
 
Other Information