Chemical Composition
0.1
%  (maximum)  
16
%    
1
%    
81.5 to 81.6
%    (estimate)
0.4
%    
1
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
276
MPa    
40
% strain    
150
   
 
Other Information
Annealed: 75,000 TS; 40,000 YS; 40 El; 75 RA; 150 HB; Oil treated: 90,000-103,000 TS; 50,000-98,000 YS; 25-30 El; 60-63 RA; 170-217 HB; For general fabricated stainless products; stainless; see Silcrome R.A.
NEVASTAIN, GRADE RA
 