Chemical Composition
0.15
%  (maximum)  
12 to 14
%    
83.3 to 86.7
%    (estimate)
1.25 to 2.5
%    
0.07
%  (minimum)  
P, S, or Se 0.07 min
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
276
MPa    
30
% strain    
155
   
 
Other Information
Annealed: 75,000 TS; 40,000 YS; 30 El; 60 RA; 155 HB; Cold drawn: 100,000 TS; 85,000 YS; 13 El; 50 RA; 205 HB; For screw machine products, valve trim, pump shafts; Type 416; free-cutting, stainless.