Chemical Composition
0.1
%    
16
%    
83.9
%    (estimate)
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
400
MPa    
28
% strain    
170
   
 
Other Information
Annealed: 75,000 TS; 58,000 YS; 28 El; 62 RA; 170 HB; For exterior trim, ornaments, cold rivets, tanks, retorts, nitric acid equipment; ductile, corrosion resistant.
BETHADUR NO. 430
 