Chemical Composition
0.75 to 1.5
%    
0.09
%  (maximum)  
16 to 18
%    
0.5
%  (maximum)  
70.1 to 76.8
%    (estimate)
1
%  (maximum)  
6.5 to 7.75
%    
0.04
%  (maximum)  
0.03
%  (maximum)  
1
%  (maximum)  
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 