Chemical Composition
0.08
%  (maximum)  
17 to 19
%    
65.8 to 74
%    (estimate)
2
%  (maximum)  
9 to 11.5
%    
0.035
%  (maximum)  
0.025
%  (maximum)  
1
%  (maximum)  
0.6
%  (maximum)  
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Other Information