Chemical Composition
0.45 to 0.55
%    
3 to 3.6
%    
92.6 to 94.6
%    (estimate)
0.5 to 0.8
%    
1.2 to 1.6
%    
0.03
%  (maximum)  
0.03
%  (maximum)  
0.2 to 0.5
%    
0.05 to 0.25
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 