Chemical Composition
0.0008 to 0.005
%    
0.13 to 0.2
%    
1 to 1.3
%    
96.7 to 97.9
%    (estimate)
1 to 1.3
%    
0.035
%  (maximum)  
0.035
%  (maximum)  
0.4
%  (maximum)  
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 