Chemical Composition
0.15
%  (maximum)  
0.8 to 1.2
%    
98.1 to 98.8
%    (estimate)
0.45 to 0.6
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
207
MPa    
30
% strain    
170
   
 
Other Information
Links



No warranty is given for the accuracy of these data