Chemical Composition
0.03
%  (maximum)  
17 to 19
%    
65 to 72.9
%    (estimate)
2
%  (maximum)  
0.75
%  (maximum)  
0.1 to 0.2
%    
10 to 12
%    
1
%  (maximum)  
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
270
MPa    
550 to 750
MPa    
40
% strain    
 
Other Information
Links
Organizations

 



No warranty is given for the accuracy of these data