Chemical Composition
54.7
%    (estimate)
0.3
%    
45
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
145
MPa    
30
% strain    
10
   
 
Other Information
Sheet: 65,800 TS; 21,000 YS; 30 El; 10, HB; Initial permeability 2500; max permeability 25,000. For audio frequency apparatus and output transformers; high permeability.
PERMALLOY 45
 
Links