Chemical Composition
0.8 to 1.1
%    
98.4 to 98.7
%    (estimate)
0.25
%    
0.25
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
758 to 1030
MPa    
1140 to 1490
MPa    
11 to 15
% strain    
330 to 600
   
 
Other Information
Water hardened: 166,000-216,000 TS; 110,000-150,000 YS; 11-15 El; 32-37 RA; 330-600 HB; For taps, drills, reamers, punches, stamps, knurls, mandrels. Type W1; water hardened.
ATSCO EXTRA
 