Chemical Composition
0.25 to 0.34
%    
0.8 to 1.2
%    
0.4 to 0.7
%    
0.15 to 0.35
%    
0.035
%  (maximum)  
0.4
%  (maximum)  
0.15 to 0.4
%    
 