Chemical Composition
0.06
%    
99.5
%    (estimate)
0.35
%    
0.025
%    
0.025
%    
0.05
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
172
MPa    
28
% strain    
 
Other Information
Plate: 35,000 TS; 25,000 YS; 28 El. For magnet cores in linear accelerators, cyclotrons, synchrotrons, bubble chambers. Soft magnet steel; high permeability, high flux density, low hysteresis loss.
LUKENS HP
 
Links
 



No warranty is given for the accuracy of these data