Chemical Composition
0.03
%  (maximum)  
0.09 to 0.14
%    
0.12
%  (maximum)  
0.17
%  (maximum)  
97.4 to 98.5
%    (estimate)
0.85 to 1.15
%    
0.48 to 0.62
%    
0.12
%  (maximum)  
0.02
%  (maximum)  
0.02
%  (maximum)  
0.08 to 0.22
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 