Chemical Composition
0.38
%    
5.1
%    
91.8
%    (estimate)
1.3
%    
1
%    
0.4
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
229
   
 
Other Information
DIN X38CrMoV51; WNr. 1.2343. Soft annealed, max 229 HB; Hot working tools in die forging presses for steels and light metals, in forging machines and extrusion presses; pressure casting dies for light metals; plastic moulds.
KRUPP 2343
 