Chemical Composition
0.4
%    
0.8 to 1.1
%    
98.2 to 98.7
%    (estimate)
0.15 to 0.25
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
655
MPa    
15
% strain    
270
   
 
Other Information
Rolled: 130,000 TS; 95,000 YS; 15 El; 40 RA; 270 HB; Annealed: 90,000 TS; 65,000 YS; 27 El; 55 RA; 185 HB; For gears, shafts, axles, fittings, bolts; oil hardened.
ARISTOLOY 4140
 



No warranty is given for the accuracy of these data