Chemical Composition
0.15
%  (maximum)  
1.45 to 2
%    
97.1 to 98
%    (estimate)
0.6 to 0.8
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
172
MPa    
30
% strain    
170
   
 