Chemical Composition
0.9
%    
18
%    
80.9
%    (estimate)
0.2
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
1860
MPa    
1930
MPa    
3
% strain    
555
   
 
Other Information
Annealed: 110,000 TS; 65,000 YS; 18 El; 35 RA; 220 HB; Heat treated: 280,000 TS; 270,000 YS; 3 El; 15 RA; 555 HB; For cutlery, valves, ball bearings, surgical instruments; corrosion and wear resistant, hardenable.
CROMINO 8M
 