Chemical Composition
0.4
%    
1.4
%    
94.3
%    (estimate)
0.4
%    
3.5
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
634 to 786
MPa    
993 to 1080
MPa    
10 to 12
% strain    
32 to 280
   
 
Other Information
Heat treated: 144,000-156,000 psi TS; 92,000-114,000 psi YS; 10-12 El; 280-32 HB; For gears, shafts, countershafts, mining equipment; oil hardened, tough, shock resistant.
MANOIR ABRADUR 500
 