Chemical Composition
95.7 to 97.6
%    (estimate)
0.9 to 1.25
%    
0.03
%    
0.02
%  (maximum)  
1.5 to 3
%    
4.0 TC approx
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 