Chemical Composition
0.18
%    
97.9 to 99.8
%    (estimate)
1.35
%  (maximum)  
0.55
%  (maximum)  
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
324
MPa    
490 to 565
MPa    
26 to 100
% strain    
 
Other Information
Rolled plate: 71,000-82,000 TS; 47,000 YP min; 26 El min. For ship plate, oil tankers, thermal power generating equipment, mine cars, bus bodies. Constructional steel plate, tough.
WELCON 50
 
Links
 