Chemical Composition
0.12
%    
9
%    
71.9
%    (estimate)
19
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
372
MPa    
42
% strain    
128
   
 
Other Information
Annealed: 76,500 TS; 54,000 YS; 42 El; 50 RA; 128 HB; For chemical plants; not used for atmospheric corrosion; corrosion resistant to sulfuric acid and HCl.
BETHADUR NO. 3
 
Links