Chemical Composition
0.35
%    
0.45
%    
96.8
%    (estimate)
0.8
%    
0.6
%    
1
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
621
MPa    
20
% strain    
241
   
 
Other Information
Heat treated: 140,000 TS; 120,000 YS; 18 El; 50 RA; 321 HB; At 1000 F: 110,000 TS; 90,000 YS; 20 El; 70 RA; 241 HB; For bolts, studs, forgings; creep resistant, oil hardened.