Chemical Composition
0.1
%    
99.9
%    (estimate)
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
296
MPa    
38
% strain    
77
   
 
Other Information