Chemical Composition
94.8
%    (estimate)
0.1
%    
4
%    
0.5
%    
0.6
%    
Al is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
207 to 248
MPa    
379 to 427
MPa    
18 to 25
% strain    
93 to 100
   
 
Other Information
Annealed: 25,000 TS; 14 El; 60 HB; Heat treated: 55,000-62,000 TS; 30,000-36,000 YS; 18-25 El; 93-100 HB; For light alloy parts for automobiles, airplanes, dirigibles; age-hardening; sheet grade.
BAUSH DURALUMIN GRADE B
 