Chemical Composition
89.2 to 96.5
%    (estimate)
2.5 to 5
%    
0.2 to 1.8
%    
0.3 to 1.5
%    
0.5 to 2.5
%    
Sn, Cd, Bi
Al is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
393
MPa    
130
   
 
Other Information
Annealed: 27,000 TS; 11,000 YS; 22 El; 47 HB; Heat treated: 72,000 TS; 57,000 YS; 130 HB; For screw machine products, aircraft parts; free-cutting, age-hardenable.
SPANAL 320
 