Chemical Composition
0.015
%  (minimum)  
0.18
%  (maximum)  
2.1
%  (maximum)  
0.09
%  (maximum)  
0.03
%  (maximum)  
0.03
%  (maximum)  
0.5
%  (maximum)  
0.22
%  (maximum)  
 
Mechanical Properties
700
MPa    
750 to 900
MPa    
10
% strain    
 
Other Information